forgot to add - unless significant stress releasing is conducted - heat treated is more brittle then untreated.
an excellent paper on the subject:
http://iafss.org/publications/fss/8/211/view
key point on page 2: Proof stress and tensile strength at 600°C are 0.3-0.4 times those at room temperature.